Dow 5E16S Polypropylene Homopolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 5E16S Polypropylene Homopolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewConsistent processabilitySuperior impactGood mold releaseContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aComplies with Canadian HPFB No ObjectionDOW 5E16S Polypropylene Resin is intended for use in injection molding processes. It is a controlled rheology grade, designed for excellent impact and toughness.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
ASTM D790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: