Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 31.7 MPa | 4600 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPH-30T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Entec Hypel® PEHD.8/.962 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Ineos R12C-00 Polypropylene Random Copolymer Grade R12C-00 is a high clarity, medium flow rate random copolymer with low antistat for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Foo.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Ineos R35C-00 Polypropylene Random Copolymer Grade R35C-00 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Ineos R35C-01 Polypropylene Random Copolymer Grade R35C-01 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Global TPP-130 30% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Spartech Centrex SP-6710 Weatherable Sheet Description: Weatherable SheetCentrex is a registered trademark of Bayer Corporation.Information provided by Spartech. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Spartech PP5210 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Spartech Royalite R84/21 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite Propionate 350E0096912 Natural, Trsp Cellulose Acetate Propionate Plasticizer 13%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Engineered Plastics EPABS 19 ABS Extrusion Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Dow 5E16S Polypropylene Homopolymer Resin OverviewConsistent processabilitySuperior impactGood mold releaseContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aComplies with Canadian HPFB No ObjectionDOW 5E16S Polypr.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Dow H533-35RGU Polypropylene Homopolymer Resin OverviewExcellent spinnabilityConsistent processingAnti-gas-fadingUV resistantComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW H533-35RGU Polypropylene Resin is a controlled rheology grade intended.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Entec Hypel® PEHD.7/.962 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | D638 |
Ineos H03W-00 Polypropylene Homopolymer Grade H03W-00 is a homopolymer designed for extrusion processing. It exhibits low water carry over. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 C.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |