Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.35 GPa | 196 ksi | |
Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour sc.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | Tangent; 1.3 mm/min; ISO 178 |
Mytex Polymers AS33L-16 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L-16 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and goo.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | Tangent, 1.3 mm/min; ASTM D790 |
Flint Hills P6G2N-095 Impact Copolymer Polypropylene Features: Excellent stiffness and impact resistance, nucleated, suitable for retort and hot fill applications. Product does not contain animal derived components.Applications: Blow molding, sheet/.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Iran Petrochemical (PCC) 52518 High Density Polyethylene 52518 is a HDPE copolymer for injection molding applications requiring a good balance between easy of process, flow and mechanical properties. Application: housewares, high fluidity, injection moldi.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP2020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Copolymer Uses: Furniture Forms: PelletsInformation Provided .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | 1mm/min; ISO 178 |
Borealis BL2571 High Density Polyethylene BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | 2mm/min; ISO 178 |
Borealis Daploy™ WB180HMS Polypropylene Daploy™ WB180HMS is a propylene-based, structurally isomeric polymer.Information provided by Borealis AG |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Total PPC 5720WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 7652 is a nucleated and antistatic heterophasic copolymer with a Melt Flow index of 16 g/10 min.Polypropylene PPC 7652 is a medium flow grade intended for a wide range of injection.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Total PPH 4030 Polypropylene Homopolymer Polypropylene PPH 4030 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4030 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | At 1 mm/min; ISO 178 |
Borealis Borstar® BB2581 HDPE for Blow Molding Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM-D790 |
Polyram RamOfin RPPC711 Polypropylene, UV Stabilized UV stabilized polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
ExxonMobil Exxtral™ LNT 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high heat ageing resistance, high transparency, low color and low discoloration for contact with hot water, hot air and detergent.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | Secant; ISO 178 |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790A |
Dow 5E16S Polypropylene Homopolymer Resin OverviewConsistent processabilitySuperior impactGood mold releaseContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aComplies with Canadian HPFB No ObjectionDOW 5E16S Polypr.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790A |
Dow H533-35RGU Polypropylene Homopolymer Resin OverviewExcellent spinnabilityConsistent processingAnti-gas-fadingUV resistantComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW H533-35RGU Polypropylene Resin is a controlled rheology grade intended.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 527 |
Dow INSPIRE™ 112 Performance Polymer INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, Conditioned Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
ExxonMobil PP1364E2 Polypropylene Homopolymer Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc.. |