Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY™ EG 8185 Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a lower density POP polymer exhibiting high elasticity for fibers.Information provided by Dow
Physical Properties Metric English Comments
Density 0.885 g/cc
0.0320 lb/in³
ASTM D792
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
Dow Method