Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 83.0 °C | 181 °F | Internal Method |
Polimeri Europa Greenflex® ML 50 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 50 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 50 show high elasticity.Main Applications: Greenflex.. |
|||
Melting Point | 83.0 °C | 181 °F | Internal Method |
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green.. |
|||
Melting Point | 83.0 °C | 181 °F | DSC |
Westlake EMAC® SP2209 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Melting Point | 83.0 °C | 181 °F | DSC; ASTM D3418 |
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Melting Point | 83.0 °C | 181 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 83.0 °C | 181 °F | Exxon Method |
ExxonMobil Iotek® 7010 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Melting Point | 83.0 °C | 181 °F | Exxon Method |
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Melting Point | 83.0 °C | 181 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5003 1000 Micron EVA Powder Description: ICOFLO 510-5003 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Melting Point | 83.0 °C | 181 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,.. |
|||
Melting Point | 83.0 - 92.0 °C | 181 - 198 °F | |
Indium Corp. Indalloy 34 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 6.5 wt% Methacrylic Acid.Nucrel® 0609HSA is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment.. |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Nucrel® 30907 Ethylene Acid Copolymer Resin Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin.. |
|||
Melting Point | 83.0 °C | 181 °F | TRN-14 |
Tipco Tipcolite® TCF 1132 - CNSL+Mineral Modified Phenolic Resin having 36mm Norton Flow with 7% Hexamine CNSL/Mineral Modified Phenolic Resin having 36mm Norton Flow, in Powder FormApplications: Nitrile RubberProcessing: CompoundingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Melting Point | 83.0 °C | 181 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® .. |
|||
Melting Point | 83.0 °C | 181 °F | Dow Method |
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP) AFFINITY™ EG 8185 Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a lower density POP polymer exhibiting high elasticity for fibers.Information provided by Dow |
|||
Melting Point | 82.8 °C | 181 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® UL 7520 Adhesive Application Resin Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealan.. |
|||
Melting Point | 83.0 °C | 181 °F | DSC |
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of .. |
|||
Melting Point | 83.0 °C | 181 °F | ASTM-D3418 |
Braskem Evateno® HM 150 EVA Hot Melt Copolymer Evateno® HM 150 is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content, very low molecular weight, and easy crosslinkability. Evateno® HM-150 offers good compatibility wi.. |
|||
Melting Point | 83.0 °C | 181 °F | by DSC |
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to .. |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinue 6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin.. |
|||
Melting Point | 83.0 °C | 181 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0903B Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 9 wt% Methacrylic Acid.Nucrel® 0903B is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion processes designed to process polyethylene re.. |