Material Notes:
BETAPHON™ 2 is an extrudable vibration damping coating. It can be applied robotically to oily metal panels in critical areas where high vibration damping is required, such as doors or roofs. It offers an automated alternative in the body shop or stamping plant to manually applied damping pads. Information provided by Dow
Physical Properties Metric English Comments
Solids Content >= 99 %
>= 99 %
3 hr @ 105°C
Viscosity Measurement 20

@Temperature 23.0 °C
20

@Temperature 73.4 °F
[g/min] Extruding Viscosity (Severs/Press flow; 5mm orifice, @ 43 psi)
70

@Temperature 45.0 °C
70

@Temperature 113 °F
[g/min] Extruding Viscosity (Severs/Press flow; 5mm orifice, @ 43 psi)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
30 min
Descriptive Properties Value Comments
Damping Performance: Composite Loss Factor 0.192
SAE J 1637, 2 mm thick, 10°C