Dow C759-21NA Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C759-21NA Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldable crates and boxes. The molding ease of this product enables short cycle times.High stiffnessMedium impact copolymerContains nucleating additiveContains an antistatic additiveApplications include housewares, material handling, and appliance componentsComplies with: U.S. FDA FCN 843, Europe EU-Directive 2002/72/EC food regulations, Canadian HPFB No ObjectionDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.2 MPa
3950 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Izod Impact, Notched 0.480 J/cm

@Temperature -20.0 °C
0.899 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.854 J/cm

@Temperature 23.0 °C
1.60 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Unannealed; ASTM D648