Dow Corning 3-6371 UV GEL

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3-6371 UV GEL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, translucent amber, UV cure with moisture secondary cure (for shadow areas).Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Viscosity 910 cP
910 cP
dynamic
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm >= 140
>= 140
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -80.0 °C
-112 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+12 ohm-cm
1.90e+12 ohm-cm
Dielectric Constant 2.81

@Frequency 100 Hz
2.81

@Frequency 100 Hz
2.81

@Frequency 100000 Hz
2.81

@Frequency 100000 Hz
Dielectric Strength 11.8 kV/mm
300 kV/in
Dissipation Factor <= 0.00010

@Frequency 100000 Hz
<= 0.00010

@Frequency 100000 Hz
0.0050

@Frequency 100 Hz
0.0050

@Frequency 100 Hz
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance translucent
Color amber
Flowable yes
Gel Hardness (Grams/Penetration) 40
Self Leveling yes
Water Resistant yes
Working Time (min) 10080