Dow Corning EP-9215 Cosmetic Powder

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning EP-9215 Cosmetic Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hard white elastomeric silicone powder that provides a silky and powdery skin feel, along with oil and sebum absorption. It also improves color intensity and coverage in pressed powder formulations.INCI Name: Dimethicone / Vinyl Dimethicone CrosspolymerInformation provided by Dow Corning
Physical Properties Metric English Comments
Volatiles <= 2.0 %
<= 2.0 %
Particle Size 2.0 - 7.0 µm
2.0 - 7.0 µm
Processing Properties Metric English Comments
Shelf Life 27.0 Month
27.0 Month