Physical Properties Metric English Comments
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d90
Magyar Aluminum ALO-DN-2S Alumina
Reactive Alumina
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d50
Magyar Aluminum ALO-DN-4F Alumina
Ground Alumina
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d50
Magyar Aluminum ALO-DN-4S Alumina
Ground Alumina
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d90
Magyar Aluminum ALO-EL-2S Alumina
Reactive Alumina
Particle Size 3.0 - 7.0 µm
3.0 - 7.0 µm
d50
Magyar Aluminum ALO-EL-4F Alumina
Ground Alumina
Particle Size 3.0 - 7.0 µm
3.0 - 7.0 µm
d50
Magyar Aluminum ALO-EL-4S Alumina
Ground Alumina
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d50
Magyar Aluminum ALO-G4-4G Alumina
Ground Alumina
Particle Size 4.5 - 7.0 µm
4.5 - 7.0 µm
Laser Diffraction D50
H.C. Starck High Vacuum 250 Titanium Carbide, TiC
Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC)
Particle Size 4.5 - 7.0 µm
4.5 - 7.0 µm
Laser Diffraction D50
H.C. Starck Standard 250 Titanium Carbide, TiC
Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC)
Particle Size 2.0 - 7.0 µm
2.0 - 7.0 µm
Dow Corning EP-9215 Cosmetic Powder
A hard white elastomeric silicone powder that provides a silky and powdery skin feel, along with oil and sebum absorption. It also improves color intensity and coverage in pressed powder formulation..
Particle Size 5.0 - 7.0 µm
5.0 - 7.0 µm
Grain Size; Intercept Method
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Grain Size; Intercept Method
CoorsTek ADS-96R 96% Alumina Thick Film Substrate
This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Chesterton 725 Nickel Anti-Seize Compound
Description: Chesterton® 725 Nickel Anti-Seize Compound is an assembly lubricant combining the extreme pressure, corrosion resistant anti-seize abilities of colloidal nickel, aluminum and graphite ..
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Chesterton 772 Premium Nickel Anti-Seize Compound
Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipm..
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Chesterton 710 Anti-Seize Compound
Description: Chesterton® 710 Anti-Seize Compound is an anti-seize compound and assembly lubricant combining the high temperature, extreme pressure, and corrosion resistant properties of colloidal c..
Copyright © lookpolymers.com All Rights Reserved