Dow Corning FS 1265 Fluid, 300 CST

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning FS 1265 Fluid, 300 CST.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100% active, fluorosilicone polymer.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc

@Temperature 25.0 °C
1.27 g/cc

@Temperature 77.0 °F
Viscosity Measure 300 cSt
300 cSt
Kinetic/Kinematic
Surface Tension 25.7 dynes/cm
25.7 dynes/cm
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Closed cup
>= 245 °C
>= 473 °F
Open cup
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Hydrophobic Yes