Material Notes:
Two-part, transparent, medium modulus LED encapsulant with very low viscosity, very long working time, and high transparency.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength, Ultimate 0.5000 MPa
72.52 psi
Tensile Strength, Yield 1.1000 MPa
159.54 psi
at 150% elongation, maximum
Elongation at Break 60 %
60 %
Optical Properties Metric English Comments
Refractive Index 1.396
1.396
1.404
1.404
1.394

@Wavelength 1554 nm
1.394

@Wavelength 1554 nm
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Mix Ratio (X:1) 100
Base to Catalyst ETN