Material Notes:
DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offer good melt strength for high throughput rates.Information provided by Dow
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Thickness 20.3 microns
0.800 mil
Melt Flow 0.85 g/10 min
0.85 g/10 min
ASTM D1238
Antiblock Level 5000 ppm
5000 ppm
Slip Level 900 ppm
900 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.4 MPa
1650 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.51 MPa
1525 psi
ASTM D882
Film Elongation at Break, MD 370 %
370 %
ASTM D882
Film Elongation at Break, TD 620 %
620 %
ASTM D882
Elmendorf Tear Strength MD 300 g
300 g
ASTM D1922
Elmendorf Tear Strength TD 475 g
475 g
ASTM D1922
Elmendorf Tear Strength, MD 14.8 g/micron
375 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 23.376 g/micron
593.75 g/mil
ASTM D1922
Dart Drop Test 400 g
0.882 lb
Method A; ASTM D1709
Film Tensile Strength at Break, MD 46.9 MPa
6800 psi
ASTM D882
Film Tensile Strength at Break, TD 42.7 MPa
6200 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
Dow Method (DSC)
Copyright © lookpolymers.com All Rights Reserved