Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 900 ppm | 900 ppm | |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Slip Level | 900 ppm | 900 ppm | |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Slip Level | 900 ppm | 900 ppm | |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
Slip Level | 900 ppm | 900 ppm | |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Slip Level | 900 ppm | 900 ppm | |
Dow DOWLEX™ 2020G Linear Low Density Polyethylene DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput.. |