Material Notes:
OverviewExcellent spinnabilityConsistent processingAnti-gas-fadingUV resistantComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW H533-35RGU Polypropylene Resin is a controlled rheology grade intended for use in fiber spinning applications requiring fine denier where UV and anti-gas-fading are desired.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
ASTM D790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: