Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow SPECFLEX™ NC 630 Polyol

Category Polymer
Manufacturer Dow Chemical
Trade Name SPECFLEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow SPECFLEX™ NC 630 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082-00-2 026301-10-0Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.022 g/cc
1.022 g/cc
Viscosity Measure 80 cSt

@Temperature 98.9 °C
80 cSt

@Temperature 210 °F
600 cSt

@Temperature 37.8 °C
600 cSt

@Temperature 100 °F
1250 cSt

@Temperature 25.0 °C
1250 cSt

@Temperature 77.0 °F
7200 cSt

@Temperature 0.000 °C
7200 cSt

@Temperature 32.0 °F
Maximum Moisture Content 0.060
0.060
wt% water
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 1.84 J/g-°C

@Temperature 20.0 °C
0.440 BTU/lb-°F

@Temperature 68.0 °F
1.99 J/g-°C

@Temperature 60.0 °C
0.476 BTU/lb-°F

@Temperature 140 °F
2.09 J/g-°C

@Temperature 100 °C
0.500 BTU/lb-°F

@Temperature 212 °F
Thermal Conductivity 0.161 W/m-K
1.12 BTU-in/hr-ft²-°F
0.154 W/m-K

@Temperature 100 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.159 W/m-K

@Temperature 50.0 °C
1.10 BTU-in/hr-ft²-°F

@Temperature 122 °F
Flash Point >= 204 °C
>= 399 °F
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 29 - 33