Polymer Property : Thermal Conductivity = 1.07 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.154 W/m-K
1.07 BTU-in/hr-ft²-°F
ASTM D2214
Lord Adhesives Thermosetâ„¢ SC-300M Silicone Gel Encapsulant
SC-300M is a two-part, rapid curing, platinum-catalyzed, addition cured, silicone gel. It has an extremely soft, gel-like consistency when cured, and has excellent unprimed adhesion to most substrat..
Thermal Conductivity 0.154 W/m-K
1.07 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T85 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content
Thermal Conductivity 0.154 W/m-K
1.07 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T85 XF Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 130°Cbetter flow than T85PreprocessingMax. Water content
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.154 W/m-K

@Temperature 100 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
Dow SPECFLEX™ NC 630 Polyol
SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082..
Thermal Conductivity 0.155 W/m-K

@Temperature 100 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Thermal Conductivity 0.154 W/m-K

@Thickness 6.35 mm,
Temperature 44.3 °C
1.07 BTU-in/hr-ft²-°F

@Thickness 0.250 in,
Temperature 112 °F
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..