Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q50Y Polyurethane Rubber Yellow/Green Polyurethane Rubber, 50-60 °IRHD. ASTM & ISO designation = AU.Applications: Good abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyuretha.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70R Polyurethane Rubber Peroxide cured, red Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion r.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70W Polyurethane Rubber Peroxide cured, off-white Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abra.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70X Polyurethane Rubber Peroxide cured, self-lubricating, Polyurethane Rubber, 65-75 °IRHD. Compounded with graphite or molyb-d. To meet ASTM line call-out M5BG714, B14, EO14, EO34. Polyester-based urethane. ASTM & ISO d.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q75B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG728, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q80Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 75-85 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG814, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q90B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Indium Corp. Indalloy® 84001 Flux #1 Paste Flux containing Ammonium Chloride Indalloy Flux #1 is a non-acid, non toxic, Pb-free, amber colored paste flux for use on copper, brass, galvanized iron, lead, zinc, tin, silver, nickel, mild steel, terne plate and malleable iron. .. |
|||
Flash Point | >= 204 °C | >= 399 °F | ASTM D92 |
ExxonMobil Mobil Almo 527 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® E-14 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: The Epolene E-14 is a low molecular-weight, low-density, oxidized polyethylene. It is useful as a lubricant in processing rigid and flexible polyvinyl chloride (PVC) and as a pr.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® E-14EP Oxidized Low Molecular Weight Polyethylene Polymer Description: The Epolene E-14EP is a low molecular weight, low density, oxidized polyethylene powder. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Flash Point | 204 °C | 399 °F | [°C] Fire Point |
ChevronTexaco Canopus® 13 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco ECO® ISO 32 Hydraulic Oil AW FeaturesChevron ECO Hydraulic Oils AW are environmentally responsible hydraulic oils.They are manufactured from high viscosity index re-refined paraffinic base oils.They provide antiwear protection,.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco RPM® SAE 75W-90 Synthetic Gear Lubricant FeaturesChevron RPM Synthetic Gear Lubricant is a heavy duty, extreme pressure, multigrade automotive gear lubricant.It is manufactured from synthesized hydrocarbon base fluids which have excellent .. |
|||
Flash Point | 204 °C | 399 °F | |
ChevronTexaco Syn-Star® GL SAE 75W-90 Texaco Syn-Star GL oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in these products provides outstanding stability.Extended drain cap.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Closed Cup; ASTM D93 |
Dow PAPI™ 95 Polymeric MDI PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Dow SPECFLEX™ NC 630 Polyol SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 783-2 Series Synthetic Food Grade Greases, NLGI Grade 2 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco Dura-Lith® NLGI 0 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Closed Cup; ASTM D93 |
Dow PAPI™ 20 Polymeric MDI PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Closed Cup; ASTM D93 |
Dow PAPI™ 580 N Polymeric MDI PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi.. |
|||
Flash Point | >= 204 °C | >= 399 °F | ASTM D92 |
ExxonMobil Mobil Almo 527 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |