Material Notes:
SPECTRIM™ 50-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D412
Elongation at Break 190 %
190 %
ASTM D412
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
Tear Strength 109 kN/m
620 pli
ASTM D624
Heat Distortion 240 %
240 %
4" Heat sag - 250°F / 60 min (1/8" thickness); ASTM D3769
Processing Properties Metric English Comments
Mold Temperature 62.8 - 73.9 °C
145 - 165 °F
Injection Pressure 9.65 - 17.2 MPa
1400 - 2500 psi
Gel Time 0.0200 min
0.0200 min