Polymer Property : Flexural Modulus = 0.345 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.345 GPa
50.0 ksi
ISO METHOD 178
NYCOA 2263 Copolymer Nylon Alloy
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Flexural Modulus 0.345 GPa
50.0 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), 1 % Secant; ASTM D790
Network Polymers NPP 11-3225
Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc.
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer.
Flexural Modulus 0.345 - 5.85 GPa
50.0 - 848 ksi
Average value: 2.37 GPa Grade Count:18
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin  (discontinued **)
Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic..
Flexural Modulus 0.345 GPa
50.0 ksi
1% Secant, 0.05 in/min; ASTM D790
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'..
Flexural Modulus 0.345 GPa
50.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als..
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
Dow SPECTRIM™ 50-S Reaction Moldable Polymer
SPECTRIM™ 50-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p..
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
Techmer ES HiFill® TPU 0600
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin  (discontinued **)
Good processability, Excellent impact resistance, Excellent flexibility and freedom from warpageApplications: Automotive splash-guards, Large containers, Closures and lids for food applicationsAddit..