Dow Tyril® 1011 SAN

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent
Manufacturer Dow Chemical
Trade Name Tyril®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Tyril® 1011 SAN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TYRIL® 1011 SAN copolymer is a light stabilized general purpose injection molding resin available in crystone color only. It exhibits excellent weathering characteristics, high strength, good chemical resistance and excellent processability.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM Data
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM Data
Elongation at Break 2.2 %
2.2 %
ASTM Data
Tensile Modulus 3.45 GPa
500 ksi
ASTM Data
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO Data
2.00 J/cm²
9.52 ft-lb/in²
ISO Data, Low Temp
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO Data
0.200 J/cm²
0.952 ft-lb/in²
ISO Data, Low Temp
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C

@Temperature 20.0 °C
37.2 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Unannealed; ASTM Data
Vicat Softening Point 104 °C
219 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Oxygen Index 18.5 %
18.5 %
Optical Properties Metric English Comments
Haze 0.80 %
0.80 %
Transmission, Visible 87.8 %
87.8 %