Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.Applications: Bynel® 3101, 3120, and E326 adhere to a wide variety of materials. They are most often used to adhere to PE, acid copolymers, and ionomers. In addition, Bynel® 3101 and Bynel® 3120 bond to PVDC. Bynel® 3101 is also useful in adhering to polyester. Bynel® E326 also bonds to paper. The use of Bynel® Series 3100 resins can be advantageous in applications where acid-containing polymers, such as acid copolymers or ionomers, are to be combined with PVDC. Bynel® 3101, 3120, and E326 can be used in coextrusion processes including: blown film, cast film/sheet, extrusion coating, thermal lamination. Bynel® 3101 and Bynel® 3120 can also be used in blow molding.Physical properties of Bynel® Series 3100 resins are typical of EVA resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process. Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D792
Viscosity 500000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
500000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
Melt Flow 8.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 67.0 °C
153 °F
Freezing point via DSC/ASTM D3418
87.0 °C
189 °F
Melting point via DSC/ASTM D3418
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
Nozzle Temperature 235 °C
455 °F
Die
Users viewing this material also viewed the following: