Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 127UV BK701 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV Stabilized High Viscosity Acetal Homopolymer Delrin 127UV BK701 is a high viscosity UV stabilized acetal homopolymer. It has excellent impact strength UV resistance and thermal stability. It is well suited for automotive interior applications.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.5 MPa
10400 psi
ISO 527-1/-2
Elongation at Break 37 %
37 %
Nominal; ISO 527-1/-2
Elongation at Yield 22 %
22 %
ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1/-2
Flexural Modulus 2.80 GPa
406 ksi
ISO 178
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
324 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >POM<
ISO 11469
Processing Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM
ISO 1043
Special Characteristics Light stabilised or stable to light
U.V. stabilised or stable to weather
UL recognition UL