DuPont Performance Polymers Hytrel® 52FR Polyester Elastomer TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® 52FR Polyester Elastomer TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Concentrate in 55 Shore D Polyester Elastomer Carrier Developed for Improving Flame RetardancyInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
ISO 1183
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Processing Casting
Coatable
Film Extrusion
Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America