Material Notes:
Activator for structural Adhesives and anaerobics. Solvent free.
Physical Properties Metric English Comments
Viscosity 100 - 200 cP
100 - 200 cP
Processing Properties Metric English Comments
Cure Time <= 1.00 min
<= 0.0167 hour
on metal (Fixture)
1440 min
24.0 hour
On metal (Full)
Descriptive Properties Value Comments
Color Brown