DuPont Performance Polymers Hytrel® HTR8241 TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8241 TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent oil, hydraulic fluids and grease resistance.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Melt Flow 4.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D <= 65
<= 65
ISO 868
63

@Time 15.0 sec
63

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Stress 17.6 MPa

@Strain 10.0 %,
Temperature 23.0 °C
2550 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
Elongation at Break 265 %

@Temperature 23.0 °C
265 %

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Modulus 0.340 GPa

@Temperature 23.0 °C
49.3 ksi

@Temperature 73.4 °F
ISO 527
Flexural Modulus 0.325 GPa

@Temperature 23.0 °C
47.1 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -40.0 °C
5.23 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
NB

@Temperature 0.000 °C
NB

@Temperature 32.0 °F
ISO 180/1A
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-1/-2
Brittleness Temperature <= 70.0 °C
<= 158 °F
ISO 974
Processing Properties Metric English Comments
Melt Temperature 235 °C
455 °F
Optimum; Extrusion
245 °C
473 °F
Optimum; Injection Molding
Mold Temperature 45.0 °C
113 °F
optimum; Injection Molding
45.0 - 55.0 °C
113 - 131 °F
Injection Molding
Drying Temperature 100 °C
212 °F
Extrusion
100 °C
212 °F
Injection Molding
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Extrusion
2.00 - 3.00 hour
2.00 - 3.00 hour
Injection Molding
Moisture Content <= 0.080 %
<= 0.080 %
Extrusion
<= 0.080 %
<= 0.080 %
Injection Molding
Descriptive Properties Value Comments
Generic TPC-ET
Part Marking Code >TPC-ET<
ISO 11469
Product Category Extrusion Resins
Specialty Resins
Resin Identification TPC-ET
ISO 1043