Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 °C | 212 °F | |
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 45FS GF20 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 65FS GF10 PC/ABS-blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 65H MA5 PC/ABS-blend, Low Friction Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Drying Temperature | 100 °C | 212 °F | DAM |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Requested for non-reinforced self-extinguishing types. Temperature can be reduced when using vacuum ovens. |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Drying Temperature | 100 - 110 °C @Time 7200 - 14400 sec |
212 - 230 °F @Time 2.00 - 4.00 hour |
Pre-drying |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Drying Temperature | 100 °C | 212 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Drying Temperature | 100 - 110 °C @Time 14400 - 21600 sec |
212 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Drying Temperature | 100 °C | 212 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Drying Temperature | <= 100 °C | <= 212 °F | |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | |
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Drying Temperature | 100 °C | 212 °F | |
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | Injection Molding |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Drying Temperature | 100 °C | 212 °F | |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Drying Temperature | 100 °C | 212 °F | |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Pre-drying Temperature |
Asahi Kasei Xyron® A0100 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Requested for non-reinforced self-extinguishing types. Temperature can be reduced when using vacuum ovens. |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |