Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 °C | 212 °F | |
PolyOne OnFlex™ S KA 60A-3S1769 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend C65HF PC/ABS-blend Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Requested for non-reinforced self-extinguishing types. Temperature can be reduced when using vacuum ovens. |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Drying Temperature | 100 - 110 °C @Time 14400 - 21600 sec |
212 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation .. |
|||
Drying Temperature | 100 - 110 °C @Time 14400 - 21600 sec |
212 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Drying Temperature | 100 °C | 212 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Drying Temperature | 100 °C | 212 °F | |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Eurotec® Tecoform® PO20 GR10 NL HS POM, 10% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural Information provided by Eurotec® |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Eurotec® Tecoform® PO20 AR10 NL HS POM, 10% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 100 °C | 212 °F | |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Drying Temperature | 100 °C | 212 °F | |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Drying Temperature | 100 °C | 212 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Drying Temperature | 100 °C | 212 °F | |
BASF Ultraform® N2650 Z6 POM + PUR Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF |