DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polytrimethylene Terephthalate (PTT)
Manufacturer DuPont Performance Polymers
Trade Name Sorona®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for consiInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Break 15 %
15 %
Nominal; ISO 527-1/-2
Elongation at Yield 5.5 %
5.5 %
ISO 527-1/-2
Tensile Modulus 2.40 GPa
348 ksi
ISO 527-1/-2
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Part Marking Code >PTT<
ISO 11469
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PTT
Users viewing this material also viewed the following: