Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 228 °C | 442 °F | |
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn.. |
|||
Melting Point | 228 - 244 °C | 442 - 471 °F | Limits; M2E-73-002 |
Indorama Ventures Mexico Polyclear™ T-94 PET Resin Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Pocan® BF 4130 XF 700051 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowability |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 150BW Wire & Cable Low Density Polyethylene Resin Product Description: LD 150BW is a LDPE containing suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house compounding it can a.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 201.48 Low Density Polyethylene Resin Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 252 Low Density Polyethylene Resin (European Grade) Product Description: LD 525 is a high purity LDPE extrusion coating grade, designed to meet environmental needs for reduced fume emissions during plastics conversion. This grade offers:Low volatiles.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North .. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade) Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock.. |
|||
Melting Point | <= 228 °C | <= 442 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 653 Low Density Polyethylene Resin (European Grade) Product Description: LD 653 is an easy flowing LDPE grade with medium stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: .. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight w.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight .. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Unreinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renew.. |
|||
Melting Point | 228 °C | 442 °F | STN EN 11357-1 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight develo.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature condi.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions... |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a.. |
|||
Melting Point | 228 °C | 442 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad.. |
|||
Melting Point | 228 °C | 442 °F | ASTM D3417 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |