Material Notes:
DuPont Vespel TP-8212 parts are specified for high-temperature applications requiring electrical insulation. TP-8212 parts offer a unique balance of mechanical and thermal properties with a low coefficient of thermal expansions, resistance to chemicals anInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc

@Temperature 23.0 °C
1.56 g/cc

@Temperature 73.4 °F
ASTM D792
Water Absorption 0.10 %

@Temperature 23.0 °C
0.10 %

@Temperature 73.4 °F
60%RH,23°C,24h; ASTM D570
0.23 %

@Temperature 23.0 °C
0.23 %

@Temperature 73.4 °F
50%RH,23°C,24h; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 106 MPa

@Temperature 150 °C
15400 psi

@Temperature 302 °F
ASTM D638
165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
ASTM D638
4.0 %

@Temperature 150 °C
4.0 %

@Temperature 302 °F
ASTM D638
Flexural Strength 173 MPa

@Temperature 150 °C
25100 psi

@Temperature 302 °F
ASTM D790
241 MPa

@Temperature 23.0 °C
35000 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 0.00800 GPa

@Temperature 150 °C
1.16 ksi

@Temperature 302 °F
ASTM D790
0.00950 GPa

@Temperature 23.0 °C
1.38 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm

@Temperature 23.0 °C
1.00e+14 ohm

@Temperature 73.4 °F
ASTM D257
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
3.7

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
ASTM D150
3.8

@Frequency 10000 Hz,
Temperature 23.0 °C
3.8

@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
Dissipation Factor 0.0012

@Frequency 10000 Hz,
Temperature 23.0 °C
0.0012

@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
0.0036

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
0.0036

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
ASTM D150
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Material Status Current
Region Available - Global Yes
RoHS Compliance Contact Manufacturer
Users viewing this material also viewed the following: