Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Sclairfilm® MPP-1 LLDPE Film, "Super Strength", 25 µm Thickness  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding heat seal and hot tack properties of Sclairfilm®. Because of its truly exceptional puncture, impact, and tear strength characteristics, and its outstanding flex-crack resistance, Sclairfilm® MPP sealant film allows up to 50% downgauging of the sealant layer in a wide variety of packaging applications.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
Moisture Vapor Transmission 0.240 cc-mm/m²-24hr-atm
0.610 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
Water Vapor Transmission 9.40 g/m²/day
0.605 g/100 in²/day
ASTM E96 Procedure E
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 80 %
80 %
ASTM D882
Film Elongation at Break, TD 800 %
800 %
ASTM D882
Tensile Modulus 0.0200 GPa
2.90 ksi
ASTM D882
Elmendorf Tear Strength MD 200 g
200 g
ASTM D1004
Elmendorf Tear Strength TD >= 800 g
>= 800 g
ASTM D1004
Dart Drop Test 200 g
0.441 lb
Film Tensile Strength at Break, MD 82.7 MPa
12000 psi
ASTM D882
Film Tensile Strength at Break, TD 38.0 MPa
5510 psi
ASTM D882
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 90 %
90 %
20°; ASTM D2457