Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® AF Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® AF Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® AF is a clear polyester film coated both sides with an anti-fog coating. Typical Applications: Typical applications include face shields, masks, visors, and other industrial uses.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 %
150 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
ASTM D1003
Transmission, Visible 89 %

@Thickness 0.102 - 0.165 mm
89 %

@Thickness 0.00400 - 0.00650 in
TLT; ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 3099 in2/lb
650 Gauge
5035 in2/lb
400 Gauge