Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dyna-Purge® X Purging Compound

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Shuman Dyna-Purge®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dyna-Purge® X Purging Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designed for Sheet & Profile ExtrusionGeneral Description:DYNA-PURGE X is a non-abrasive, non-chemical “engineered” thermoplastic purging compound, formulated to have a natural flow through the extruder. A non-melting but softening thermoplastic scrubs the screw and barrel, while the carrier matrix flushes away impurities. The material is designed for extruders and co-extruders that process tubing or pipe, sheet, and other profiles.FEATURES & BENEFITS OF DYNA-PURGE XExcellent for color changes, resin changes, preventative machine maintenance, and before manual cleaningDeveloped for purging through the barrel, die head, and other downstream equipment with a minimum clearance of .025 inch (.65 mm)Effective through a wide temperature range 320°F to 575°F (160°C to 302°C)Easy to use – no process adjustment necessary – use at the resident resin processing temperature and RPM speedNon-abrasive, non-melting but softening thermoplastic, which thoroughly loosens carbonized and degraded resin, allowing it to be flushed out of the systemSafe, non-hazardous, with no chemicals - ingredients are FDA compliantHeat stable – recommended during shutdown and start-upLow “cost per purge” – only small quantity needed to be effectiveNo mixing required, simply use “as is”Unlimited shelf life
Processing Properties Metric English Comments
Processing Temperature 160 - 302 °C
320 - 576 °F
Extrusion
Descriptive Properties Value Comments
Amount of Purge (Extrusion) Approx. 10 lbs per diameter inch of screw
L:D dependant
Minimum Orifice (Extrusion) .025in, .65mm
Die
Screen Packs or other flow restrictions (Ext.) Combination of 20, 40, 60 or 80 mesh; 100 or more, use SF or F
Types of Resins All