Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 293 - 302 °C | 560 - 575 °F | |
Oxford Polymers Oxnilon 66-ST-30GF 30% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection Molding 30% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Injection |
Dyna-Purge® B Purging Compound Designed for Injection and Extrusion Blow MoldingGeneral Description:DYNA-PURGE B is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow naturally .. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Extrusion |
Dyna-Purge® B Purging Compound Designed for Injection and Extrusion Blow MoldingGeneral Description:DYNA-PURGE B is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow naturally .. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Injection |
Dyna-Purge® P Purging Compound Designed for Hot Runner SystemsGeneral Description:DYNA-PURGE P is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to have a natural flow through the b.. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Extrusion |
Dyna-Purge® SF Purging Compound Designed for Sheet & Profile Co-Extrusion & Multi-Layer FilmGeneral Description:DYNA-PURGE SF is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, with a proprietar.. |
|||
Processing Temperature | 160 - 302 °C | 320 - 576 °F | Extrusion |
Dyna-Purge® X Purging Compound Designed for Sheet & Profile ExtrusionGeneral Description:DYNA-PURGE X is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to have a natural flow throug.. |