Material Notes:
Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops properties of vulcanized rubber yet not requiring vulcanization. It is protected with a non staining antioxidant system; FDA approved, suitable for food contact applications and is essentially gel free with a very clear color. Solprene 416 is used as elastomeric modifier for asphalt and plastics, as ingredient of soling formulations and as base for pressure sensitive adhesives. It is available as free flowing porous crumb for easy handling and dissolution, packaged in standard paper bags, super sacs and cardboard boxes.Applications:AdhesivesPlastic modificationInformation provided by Dynasol
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
DIN-53479
Volatiles <= 0.75 %
<= 0.75 %
ASTM D-5668
Brookfield Viscosity 30000 cP
30000 cP
25% toluene solution; MA 04-3-064
Viscosity Measure 11 cSt
11 cSt
Toluene solution viscosity 5,23%; NM 300-11
Melt Index of Compound <= 0.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 0.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D-2240
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D-412
Elongation at Break 800 %
800 %
ASTM D-412
300% Modulus 0.00270 GPa
0.392 ksi
ASTM D-412
Chemical Properties Metric English Comments
Styrene Content >= 28 %
>= 28 %
Block; NM-202-07
30 %
30 %
on polymer; ASTM D-5775