Physical Properties Metric English Comments
Viscosity Measure 11 cSt
11 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 416 Styrene-Butadiene TPE Copolymer  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Thanks to its moderate molecular weight, Finaprene® 416 provid..
Viscosity Measure 11 cSt
11 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 502 Styrene-Butadiene TPE Copolymer  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 502 is a thermoplastic elastomer type linear butadiene-butadiene block copolymer (SBS). Thanks to its high styrene content, Finaprene® 502 provi..
Viscosity Measure >= 11 cSt

@Temperature 100 °C
>= 11 cSt

@Temperature 212 °F
Unipetrol Heavy Oil Hydrogenate
Oil hydrogenates are a fraction boiling at above approximately 300°C, gained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of semi-soli..
Viscosity Measure 11 cSt
11 cSt
5.23% Toluene solution; NM-300-11
Dynasol Solprene® 4301 Thermoplastic Rubber (SBS)
Solprene 4301 is a linear block copolymer of styrene and butadiene, having 33% styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a non..
Viscosity Measure 11 cSt
11 cSt
5.23% Toluene solution; NM-300-11
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Solprene 4316 is a radial styrene/butadiene block copolymer with 30% styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops propertie..
Viscosity Measure 11 cSt
11 cSt
Toluene solution viscosity 5,23%; NM 300-11
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry
Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops proper..