Material Notes:
Solprene 4316 is a radial styrene/butadiene block copolymer with 30% styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops properties of vulcanized rubber yet not requiring vulcanization. It is protected with a non staining antioxidant system; FDA approved, suitable for food contact applications and is essentially gel free with a very clear color. It is available as free flowing porous crumb for easy handling and dissolution, packaged in standard paper bags, super sacs and cardboard boxesUses: Solprene 4316 is used as elastomeric modifier for asphalt and plastics, as ingredient of soling formulations and as base for pressure sensitive adhesives.Main Applications: PavingPolymer modificationAdhesivesFootwearInformation provided by Dynasol.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
DIN 53479
Volatiles <= 0.75 %
<= 0.75 %
ASTM D5668
Viscosity Measure 11 cSt
11 cSt
5.23% Toluene solution; NM-300-11
Melt Flow <= 0.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 0.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D2240
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
300% Modulus 0.00270 GPa
0.392 ksi
ASTM D412
Chemical Properties Metric English Comments
Styrene Content >= 29 %
>= 29 %
Block; NM 202-07
30 %
30 %
on polymer; ASTM D5775