Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact, weather resistance, chemical resistanceInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 260 - 280 °C
500 - 536 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F