Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 270 - 280 °C | 518 - 536 °F | Average value: 275 °C Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Processing Temperature | 265 - 280 °C | 509 - 536 °F | Manifold |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |
|||
Processing Temperature | 180 - 280 °C | 356 - 536 °F | Molding |
Ineos Styrenics Polystyrene 476M Q598 (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Processing Temperature | 200 - 280 °C | 392 - 536 °F | |
IRPC Polimaxx Polene 1102K Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS:MONOFILAMENT/YARN/SHEET EXTRUSION AND INJECTION MOLDING COARSE TEXTILE FOR WOVEN BAGS, TARPAULINS, ROPES, STRAWS, INDUSTR.. |
|||
Processing Temperature | 250 - 280 °C | 482 - 536 °F | |
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, GOOD CLARITY, LOW NECK IN/ODOR HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED OPP FILM |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | mass temperature |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | mass temperature |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | mass temperature |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | ISBM Processing Melt Temp. |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
E-Polymers TEKAMID® TB120G15 , 15% Glass Fiber Reinforced PA6, DAM 15% Glass Fiber reinforced, Good surface Information provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Processing Temperature | 270 - 280 °C | 518 - 536 °F | |
E-Polymers TEKAMID® TA210F Fast Crystallinity PA66, DAM Fast crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | Resin Temperature |
Asahi Kasei Xyron® 300H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | Extrusion Range |
Arkema Group Rilsan® PA 11 BESNO MED Nylon 11 Rilsan® PA 11 BESNO MED is a polyamide produced from a renewable source. This grade dedicated to extrusion offers the highest quality and it is specially designed to meet the stringent requirements.. |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | |
Zhejiang Juner PC/PBT Alloy Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |