EMS-Griltech Grilon® BS 22R Nylon 6 Monofilament (Super-Set)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® BS 22R Nylon 6 Monofilament (Super-Set).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON BS 22R is a Nylon 6 based monofilament for paper machine, clothing, forming screen, and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Filament Diameter 150 - 1000 µm
150 - 1000 µm
Mechanical Properties Metric English Comments
Elongation at Break 40 - 60 %
40 - 60 %
Tenacity 0.412 - 0.500 N/tex
4.67 - 5.66 g/denier
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Shrinkage 3.00 - 6.00 %

@Temperature 180 °C
3.00 - 6.00 %

@Temperature 356 °F
Thermo Shrinkage
Descriptive Properties Value Comments
Heat Setting Super-Set