EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)

Category Polymer , Adhesive , Thermoplastic , Nylon
Manufacturer EMS-Griltech
Trade Name Griltex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent resistance and dimensional stability of the finished garment. For technical applications, GRILTEX adhesive products are used to optimize the manufacturing process for the production of automotive interior components or parts for other applications. All values were determined on dried pellets.Applications: Adhesive Films (supported), Home FurnishingBonding Properties: Paper, Wood, Polyamide, PUR (Foam), Polyolefin, LeatherData provided by EMS-Griltech.
Physical Properties Metric English Comments
Viscosity 130000 cP

@Temperature 160 °C
130000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 160 °C
80 g/10 min

@Load 4.76 lb,
Temperature 320 °F
cm<sup>3</sup>/10 min; ISO 1133
Thermal Properties Metric English Comments
Melting Point 105 - 115 °C
221 - 239 °F
DSC
Processing Properties Metric English Comments
Processing Temperature 110 - 130 °C
230 - 266 °F
Lamination Adhesive
120 - 150 °C
248 - 302 °F
Films Die Head
Die Temperature 160 - 180 °C
320 - 356 °F
Hotmelt Coating Slot Die
Roll Temperature 150 - 170 °C
302 - 338 °F
Hotmelt Coating Multi Roller
180 - 220 °C
356 - 428 °F
Engraved Roller
Descriptive Properties Value Comments
Crystallization Speed Slow
Form of Delivery Granules, Powder