Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Die Temperature | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion |
Stellarchem SV-B40D TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion |
Stellarchem SV-B80E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Die Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | Foam extrusion molding |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Die Temperature | 140 - 180 °C | 284 - 356 °F | |
Elastron® D SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureselectrical insulator with very low conductivityhas gra.. |
|||
Die Temperature | 160 - 180 °C | 320 - 356 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | |
Fainplast Compounds HAX HFX 024-15C Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linkable by heat and moisture by previous addition of a suitable catalyst masterbatch. It is recommended to s.. |
|||
Die Temperature | 150 - 180 °C | 302 - 356 °F | |
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende.. |
|||
Die Temperature | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified
(discontinued **) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |