Material Notes:
Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has been modified with graphite to provide a low coefficient of friction, is heat stabilized, easy to mould and eject from the mould tool. The special features of this product are: Low coefficient of friction Dimensional stability Low moisture absorption Easy to process Low weight and low density The inherent color of this material is grey.Application examples: This product has been developed to provide a low coefficient of friction and can be used in applications for bearings, guide sleeves and bowden cables.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
conditioned, 15s; ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
dry; ISO 527-1/-2
40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPa
6530 psi
dry; ISO 527-1/-2
50.0 MPa
7250 psi
dry; ISO 527-1/-2
Elongation at Break 40 %
40 %
conditioned; ISO 527-1/-2
40 %
40 %
dry; ISO 527-1/-2
Elongation at Yield 10 %
10 %
dry; ISO 527-1/-2
12 %
12 %
conditioned; ISO 527-1/-2
Tensile Modulus 2.00 GPa
290 ksi
conditioned; ISO 527-1/-2
2.20 GPa
319 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 21.0 kV/mm
533 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 225 V
225 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Electrical appliances
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Other Extrusion
Product Attributes Improved friction & wear properties
Special Characteristics Improved heat resistance
Improved UV resistance (outdoor use)
Light stabilized or stable to light