Material Notes:
Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Attributes: high stiffness at low weightvery low moisture absorptionelectrically conductivefavorable abrasion and wear propertieslow coefficient of thermal expansionlow mould shrinkageeasy processinggood chemical and UV resistance Grilamid LC-15H BLACK is particularly suitable for technical components in the following application fields: Sport and leisure goodsLightweight designs and prototypesTools and instrumentsConductive electrical devicesExplosion proof safety devicesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 1.1 %
1.1 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
Tensile Strength at Break 140 MPa
20300 psi
conditioned; ISO 527-1/-2
150 MPa
21800 psi
dry; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
dry; ISO 527-1/-2
4.0 %
4.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 13.0 GPa
1890 ksi
conditioned; ISO 527-1/-2
15.0 GPa
2180 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
conditioned; IEC 60093
Surface Resistance 50 ohm
50 ohm
IEC 60093
Descriptive Properties Value Comments
Electricals & Electronics Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics Anti-static
High impact or impact modified
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following: