Material Notes:
Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium carbide precipitation and its susceptibility to inter granular corrosion.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.89 g/cc
0.285 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 689 MPa
>= 100000 psi
Tensile Strength, Yield >= 379 MPa
>= 55000 psi
0.2% Offset
Elongation at Break >= 35 %
>= 35 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.7 µm/m-°C

@Temperature 20.0 - 649 °C
10.4 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 16.3 W/m-K
113 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 18 - 20 %
18 - 20 %
Iron, Fe 65.145 - 74 %
65.145 - 74 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 8.0 - 12 %
8.0 - 12 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %