PRODUCT NO.
Manufacturer
Trade Name
Osprey Metals 304L/MA Master Alloy Stainless Steel Powder (Grade 95% - 16)
Osprey Metals, Ltd.
Osprey Metals 310S Stainless Steel Powder (Grade 80% - 22)
Osprey Metals, Ltd.
Osprey Metals 316L Stainless Steel Powder (Grade 80% - 22)
Osprey Metals, Ltd.
Osprey Metals 316L/MA Master Alloy Stainless Steel Powder (Grade 95% - 16)
Osprey Metals, Ltd.
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RD Powdered Metal
PSM Industries
Pacific Sintered Metals
Pyrotek Jacketed mesh core Tadpoles
Pyrotek, Inc.
Garlock GRAPH-LOCK® 3128 HOCHDRUCK® Graphite Sheet Gasketing, Steel Reinforced
Garlock Rubber Technologies
GRAPH-LOCK®
MetalTek MTEK 25-12 Cast UNS J93503 Heat Resistant Stainless Steel
MetalTek
MTEK
MetalTek MTEK 35-15 Cast UNS N08605 Heat Resistant Stainless Steel
MetalTek
MTEK
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel
Groupe Arcelor
SIRIUS
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
Groupe Arcelor
SIRIUS
Kinetics MIM 316 Stainless Steel (Premium Grade)
Kinetics, Inc.
MetalTek MTEK 29-10 Cast UNS J93403 Heat Resistant Stainless Steel
MetalTek
MTEK
H.C. Starck Ampersint® AISI 316 L 31 µm For P/M, HIP/CIP, MIM
H.C. Starck
Ampersint®
Universal Wire Works 316L Stainless Steel Electrode
Universal Wire Works
Eagle Brass 301 Austenitic Stainless Steel, 1/4 Hardened
Eagle Brass Company
Eagle Brass 301 Austenitic Stainless Steel, Annealed
Eagle Brass Company
Eagle Brass 302 Austenitic Stainless Steel, 1/4 Hardened
Eagle Brass Company
Eagle Brass 302 Austenitic Stainless Steel, Annealed
Eagle Brass Company
Eagle Brass 316 Austenitic Stainless Steel, 1/4 Hardened
Eagle Brass Company
Eagle Brass 316L Austenitic Stainless Steel, 1/4 Hardened
Eagle Brass Company
Crucible Steel 316L Chromium-Nickel Steel
Crucible Steel
Crucible Steel 348 Chromium-Nickel Steel
Crucible Steel
Eagle Brass 304 Austenitic Stainless Steel, 1/8 Hardened
Eagle Brass Company
Eagle Brass 304L Austenitic Stainless Steel, 1/2 Hardened
Eagle Brass Company
Eagle Brass 304L Austenitic Stainless Steel, 1/8 Hardened
Eagle Brass Company
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched
Carpenter Technology Corporation (Cartech)
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 70% Cold Worked
Carpenter Technology Corporation (Cartech)
BioDur™
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density
Ametek
ATI Allegheny Ludlum 309S Austenitic Stainless Steel
ATI Allegheny Ludlum
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
ATI Allegheny Ludlum
ATI Allegheny Ludlum MINIMISER® 316/316L Stainless Steel
ATI Allegheny Ludlum
MINIMISER®
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 30% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 40% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum
ATI Allvac® Nickelvac® 304 L UNS S30403 Specialty Steel
ATI Allvac
Nickelvac®
ATI Allegheny Ludlum AM 350™ High Strength Specialty Steel Alloy, UNS S35000
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 10% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 20% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum
Ametek P304L P/M Stainless Steel, Sintered from 6.5 g/cc Green Density
Ametek
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
ATI Allegheny Ludlum
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density
Ametek
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, Annealed (UNS S30400)
ATI Allegheny Ludlum
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum
Osprey Metals 310S Stainless Steel Powder (Grade 90% - 22)
Osprey Metals, Ltd.
Ametek P316L P/M Stainless Steel, Sintered from 6.83 g/cc Green Density
Ametek