Ecomass® 2150TU85 Tungsten Powder Filled Polyamide (PA6/6), Injection Molding Grade

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 2150TU85 Tungsten Powder Filled Polyamide (PA6/6), Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tungsten Powder Filled Polyamide (PA6/6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 5.60 g/cc
5.60 g/cc
Internal Method
Linear Mold Shrinkage 0.0090 - 0.010 cm/cm
0.0090 - 0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength 43.0 MPa
6240 psi
ISO 527
Elongation at Break 9.0 %
9.0 %
ISO 527
Tensile Modulus 2.90 GPa
421 ksi
ISO 527
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Processing Properties Metric English Comments
Melt Temperature 265 - 290 °C
509 - 554 °F
Mold Temperature 65.0 - 90.0 °C
149 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 - 6 hour
4 - 6 hour
Moisture Content <= 0.20 %
<= 0.20 %
target