Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.0 - 100 °C | 149 - 212 °F | |
PolyOne Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Mold Temperature | 65.0 - 180 °C | 149 - 356 °F | Average value: 127 °C Grade Count:34 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
LATI LAXTAR G/30 30% Glass Reinforced LCP
(discontinued **) Description: Laxtar products are liquid crystal polymers (LCP). They offer exceptional performance together with increasing cost-effectiveness. Due to the outstanding fluidity at high shear rates LC.. |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | Injection |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Mold Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
Ecomass® 1850ZC84 Stainless Steel Powder Filled Polyamide (PA6), Injection Molding Stainless Steel Powder Filled Polyamide (PA6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding a.. |
|||
Mold Temperature | 65.0 °C | 149 °F | Injection Molding |
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Mold Temperature | 65.0 °C | 149 °F | Injection Molding |
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Mold Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Mold Temperature | 65.0 - 140 °C | 149 - 284 °F | Average value: 108 °C Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |