Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ASTM D955 |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ASTM D955 |
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Horizontal |
PTS POM-90 Acetal Copolymer Information provided by PTS LLC. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.022 cm/cm | 0.020 - 0.022 in/in | ASTM D955 |
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.022 cm/cm | 0.014 - 0.022 in/in | ASTM D955 |
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 3.20 mm |
0.018 - 0.022 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.022 cm/cm @Thickness 3.20 mm |
0.020 - 0.022 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.022 cm/cm | 0.014 - 0.022 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KAL22 is a compound based on Acetal Copolymer resin containing PTFE, Aramid Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Time 86400 sec |
0.018 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Asia Pacific) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Time 86400 sec |
0.018 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.022 cm/cm | 0.017 - 0.022 in/in | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 3.20 mm |
0.018 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1820-BK1(PTFE) Lubricated, Heat Stabilized Nylon 66 Description: Lubricated, Heat Stabilized Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1627-BK2 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.022 cm/cm | 0.012 - 0.022 in/in | |
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.022 cm/cm | 0.012 - 0.022 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 4.00 mm |
0.018 - 0.022 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 4.00 mm |
0.018 - 0.022 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA6 D61 PA6, Injection Molded Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Horizontal |
BLUESTAR BS090 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Horizontal |
BLUESTAR BS130 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1863-BK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | DIS 294-4 |
Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 4.00 mm |
0.018 - 0.022 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA6 D83 PA6, Injection Molded Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |